  • Bonding protocol for BioHPP – a step-by-step guide

    The step-by-step bonding protocol for BioHPP… Follow our RDT Philip Lajoie’s eight steps to ensure reliable results with BioHPP. 1. Condition the BioHPP framework Sandblast your framework with 110 μm aluminium oxide at a pressure of 2 to 3 bar. Any impurities can be removed using a clean brush, DO NOT steam clean after sandblasting. …

    Read this story
  • for2press demo at Jonathan Pattison Ceramics

    We offer all our for2press customers full training on using the machine and ongoing technical support for pressing BioHPP. Our registered dental technicians carry out the for2press demonstration on-site at your lab and verifiable CPD is available. Here is an example of a recent BioHPP case pressed at Jonathan Pattison Ceramics as part of a …